Resources / Die Casting Alloy Comparison Guide

Die Casting Alloy Comparison Guide

Aluminum, zinc and magnesium are not interchangeable. Yield strength, wall capability, corrosion and cost per part move together, and the right alloy is the one whose weaknesses the part can tolerate.

Die casting alloy comparison for aluminum and zinc Aluminum alloy comparison review
Audience
Buyers and engineers
Focus
Practical decisions
Next
DFM review
Output
Actionable checklist

Start from the property the part actually needs

Alloy selection usually starts with a strength number and ends with a finish or corrosion problem. A better sequence is to name the dominant requirement first: structural stiffness, pressure tightness, thin-wall weight, appearance, or cost at volume. Each of those points to a different family, and the secondary requirements then narrow the grade within it.

Aluminum dominates because it balances strength, weight and cost. Zinc wins where thin walls, fine detail and as-cast cosmetics matter and weight does not. Magnesium is the lightest and the most awkward: it needs tighter process control, its corrosion protection is not optional, and fewer plants run it well.

  • Structural or pressure-bearing part → aluminum, usually A380 or ADC12
  • Thin wall under 1 mm with fine detail → zinc
  • Weight-critical housing → magnesium, with a coating plan
  • Decorative as-cast surface → zinc or polished aluminum

The three families side by side

The table below is the comparison that decides most projects. It is a family-level view; the grade decides the details. What matters is the shape of the trade: aluminum gives strength per unit cost, zinc gives detail per unit wall, magnesium gives lightness at a process premium.

PropertyAluminum (A380/ADC12)Zinc (Zamak 3/5)Magnesium (AZ91D)
Density2.7 g/cm³6.6 g/cm³1.8 g/cm³
Typical wall1.5–3.0 mm0.6–1.5 mm1.2–2.5 mm
Tensile strength~290–320 MPa~280–330 MPa~230–250 MPa
As-cast tolerance±0.05 mm±0.05 mm±0.05 mm
CorrosionGood, needs finish outdoorsExcellentPoor, coating required
MachinabilityGoodExcellentExcellent
Casting temperature~650 °C~400 °C~650 °C
Relative part costBaselineHigher per kg, lower per thin partHighest
RecyclabilityHighHighHigh

Values are typical ranges for high-pressure die casting. The controlled drawing and the alloy certificate govern the actual specification.

Aluminum: A380, ADC12 and A360

A380 and ADC12 are the workhorses. They are close relatives: both are Al-Si-Cu alloys with excellent castability, good strength and moderate machinability. A380 is the common US designation and ADC12 the Japanese equivalent; a part quoted in either will usually be produced from whichever the plant has certified. They are not identical in composition, so a customer who needs a specific grade should say so on the drawing rather than accept an equivalence claim.

A360 is the choice where corrosion resistance and pressure tightness matter more than strength. It has less copper and more silicon, which improves fluidity and reduces hot cracking, at the cost of some tensile strength. Housings that see water, salt spray or a leak test often move to A360 even though the strength margin is smaller.

A413 and similar low-iron, high-silicon grades are used for thin walls and intricate parts where fluidity dominates. They are less common in structural work because the elongation and strength are lower.

  • A380 / ADC12: default for general housings, brackets and covers
  • A360: better corrosion and pressure tightness, slightly lower strength
  • A413: maximum fluidity for thin, intricate sections
  • Confirm the grade on the certificate, not by assumption

Zinc: Zamak 3 and Zamak 5

Zinc casts at around 400 °C, which is why it can fill walls of 0.6 mm and hold fine detail, sharp corners and cast lettering that aluminum cannot. It machines beautifully, takes plating and paint well, and has excellent corrosion resistance without coating. The penalty is weight: at 6.6 g/cm³ a zinc part is roughly 2.4 times the mass of the same aluminum part.

Zamak 3 is the ductile, dimensionally stable grade used for decorative and functional hardware. Zamak 5 adds copper for strength and hardness, at some cost in ductility and dimensional stability. Zamak 2 is stronger still but rarely used outside specific bearing applications because it is brittle and dimensionally less stable.

GradeCharacterTypical use
Zamak 3Ductile, stable, good platingHandles, fittings, decorative parts
Zamak 5Stronger, harder, less ductileStructural hardware, load-bearing fittings
Zamak 2Highest strength, brittleNarrow bearing and wear applications

Zinc parts are usually specified by mass and finish rather than by tolerance, because the process holds tolerance easily at these wall thicknesses.

Die casting alloy cost per part, not per kilogram

Zinc costs more per kilogram than aluminum, and a zinc part is heavier, so the material cost of a zinc part is often several times that of the aluminum equivalent. That comparison is misleading on its own. Zinc fills a thinner wall, so the part can be lighter than the naive density ratio suggests; it casts detail that aluminum would have to machine; and it needs no coating for indoor corrosion.

The honest comparison is the finished cost: material plus casting plus machining plus finishing plus scrap. A zinc part that eliminates two machining operations and a plating step can beat an aluminum part that needs both, even at a higher material price. That is why the cost question belongs with the drawing, not with the metal price page.

  • Compare finished cost: material + casting + machining + finish + scrap
  • Thin-wall zinc can be closer in mass than the density ratio implies
  • Cast detail removes machining that aluminum would need
  • Outdoor aluminum needs a coating that zinc may not

What to put on the drawing

The drawing should name the alloy, the temper or heat treatment if any, the casting tolerance standard, the finish and the test. A generic aluminum die casting note is not a specification: it leaves the alloy, the tolerance and the acceptance open, and the quote will be based on assumptions your customer never sees.

If your customer has a preferred alloy from a previous supplier, it is worth checking why. Sometimes it is a real functional requirement; sometimes it is a habit inherited from a drawing that was never reviewed. The DFM conversation is the right place to ask.

  • Alloy and grade, by standard designation
  • Heat treatment, if the part is T5 or T6
  • Casting tolerance standard and any tighter callouts
  • Finish, coating thickness and color
  • Pressure or leak test, with the acceptance criterion

Alloy comparison: where to go next

The alloy follows from the dominant requirement and the finished cost, not from a metal price list. Send the drawing with the function and the environment and the review can compare grades on the finished cost.

Related pages

Continue through the project path.

Use the internal links to connect the material, process, industry, product and RFQ pages around one project decision.

Send the drawing. Get the engineering questions first.

Include the material, annual quantity, finishing requirement, target market and delivery date. The review can start from STEP, IGS, DWG, DXF, PDF or ZIP files.

Start an RFQ
Upload drawing