Industrial pump housings and valve bodies: pressure-tight castings

An industrial pump housing and a valve body are sold on pressure, not on appearance. The casting has to be dense in one specific band, the flange has to stay flat under bolt load, and the bore has to stay aligned after two setups. Everything else follows from those three.

Alloy
A380 / ADC12
Wall
3.0–4.5 mm
Flange flatness
0.05–0.10 mm
Pressure test
100% on pressure members
Reference design

Reference design, not a delivered customer project.

This page describes a part family and the engineering decisions it forces. It is built from the geometry class and the process route, not from one customer order: no part number, customer name, delivery date, yield figure or measured result is shown.

Delivered project data is published only with the customer written authorization, and none of these images are customer photographs.

01 / Family

Two pump housing bodies, one acceptance rule: hold the pressure.

The family share a rule — the casting is only accepted if the pressure boundary is dense — and differ in which feature carries the load.

MemberAlloyTypical wallWhat decides acceptanceRelease test
Industrial pump housingA3803.5–4.5 mmPressure wall density; bore alignment to the flange face; port positionHydro or air test 100%, CMM per lot
Gear valve bodyADC123.0–4.0 mmBore alignment of the gear cavity; end-face flatness; cross-port position100% air test, CMM first article
Gear pump coverA3803.0–3.5 mmFlatness under bolt load; seal groove sectionFlatness every lot, leak test 100%
Test medium, pressure and hold time are fixed by the drawing and the applicable standard for the end product. This page does not set a pressure class.
02 / Context

Where pressure castings fail.

On a pressure casting, porosity does not have to be large to be fatal: a connected pore across a 3 mm wall leaks at 2 bar. That is why the acceptance zone is written per surface — pressure wall, seal band, bore — instead of a blanket "no porosity" note on the whole part, which in practice either scraps the die or is quietly ignored.

  • Mark the pressure boundary on the drawing, not just in the notes
  • Agree the porosity acceptance per zone at DFM: visual, X-ray or sectioning
  • Test at the pressure the part will see, not at a convenient number
03 / Design

Decisions that keep the pressure boundary dense.

These four decide whether the casting passes its first pressure test.

Gating and overflow

Gates are placed so the last metal to freeze sits in an overflow, not in the pressure wall. On a pump body that usually means gating from the flange and venting the far end of the volute.

Wall uniformity

A 4 mm wall next to a 10 mm boss feeds shrinkage straight into the wall. Bosses are cored or moved into the machined region wherever the drawing allows.

Flange stiffness

A thin flange bows when the bolts are torqued and the gasket loses compression. 8–10 mm with ribs behind it is the usual answer on a 100 mm port.

Bore alignment

Two bores on opposite faces are machined from one datum in one setup where possible; where not possible, the second setup references the first machined face, never the as-cast surface.

04 / Route

Casting, machining, then proving it holds.

The route for this family, with the stage that usually decides whether the lot ships.

StageWhat happensControl point
DFM and pressure-zone reviewPressure boundary marked, porosity acceptance and test method agreedAcceptance zone written on the drawing before tooling
Die build and T1Gating, venting and overflow placed to keep the wall dense; vacuum assist where the wall is thinT1 X-ray or section on the pressure band
MachiningFlange face, bore and seal groove from one datum; threads after facingBore alignment and flange flatness on the CMM
Pressure testHydro or air per drawing, 100% on pressure membersTest pressure, hold time and leak rate recorded per lot
Finishing and packingConversion coating or paint with threads and seal faces maskedThreads re-checked with a gauge after coating
A pressure test after coating hides coating defects inside the pressure boundary. On this family the test is run before coating and repeated after where the drawing requires it.
05 / Failure modes

The leaks that come back.

Causes behind a failed pressure test, and the design or process change that removes them.

RiskMechanismCountermeasure
Leak through the volute wallConnected porosity across a thin sectionThicken the wall to 4 mm locally, add overflow, X-ray the band
Leak at the flangeFlange distortion under bolt torqueIncrease flange thickness, add ribs, specify flatness after machining
Bore misalignmentSecond setup referenced from the as-cast faceReference the machined datum, or finish both bores in one setup
Thread leak on a portPorosity at the thread rootMachine the port and use a sealing insert, or core the boss deeper
Crack at a sharp cornerStress concentration at an internal cornerR1.5–R3 radius at rib-to-wall and boss-to-wall junctions
06 / Inspection

Accepting a pressure casting.

Inspection is arranged around the pressure boundary first, geometry second.

CharacteristicMethodFrequency
Pressure tightnessHydro or air decay per drawing100% on pressure members
Porosity in the pressure bandX-ray or destructive sectionFirst article plus periodic audit
Bore alignmentCMM against the datumFirst article and per lot
Flange flatnessCMM or surface plateEvery lot
Thread and port integrityGo/no-go gauge, seal check100% gauge
Wall thickness at the voluteUltrasonic or sectionFirst article plus periodic audit
The X-ray view and the sectioning plane are agreed with the customer at first article so a reject can be argued with evidence rather than opinion.
07 / Inputs

What a pressure casting quotation needs.

On this family the test specification matters as much as the drawing. A housing quoted without a pressure class is quoted for geometry only, and the first failed hydro test becomes a change order.

Send with the RFQ

  • Drawing with the pressure boundary and test specification
  • Medium, test pressure, hold time and allowable leak rate
  • Port standard and thread specification
  • Annual volume and whether the part is machined by us
  • Finishing requirement, including masking of threads and seal faces
  • Any end-product standard the test has to follow
Buyer questions

Pressure casting questions

The questions that decide whether a pump body or valve body is quotable.

The casting does not have a pressure rating on its own; the rating belongs to the tested assembly and to the standard it is built against. What we do is cast and machine so the pressure boundary is dense, then test to the pressure and hold time the drawing specifies, with the porosity acceptance written per zone.

Three levers: gate so the last metal freezes in an overflow rather than the wall, keep wall sections uniform so shrinkage has somewhere to go, and use vacuum assist where the wall is thin. None of them replaces the X-ray check on the first article, which is what proves the layout works.

Faced before coating, masked during coating, and verified after. A coated flange face is a gasket that creeps; a flange faced after coating is a flatness callout that no longer matches the drawing. Masking is the cheap option and it is written into the finishing specification.

On most pump bodies yes, if the part can be held from the flange while both bores are cut. Where the geometry forces two setups, the second one references the first machined face, and coaxiality is measured on the relaxed part rather than in the fixture.

Yes, per lot, with the test pressure, hold time and result, together with the dimensional report. The format is agreed at first article so it matches what the customer quality file expects.

Send the drawing and the test specification.

We answer within 30 minutes during Shenzhen business hours with a price direction or the questions we still need answered.

Start an RFQ
Upload drawing